求翻译:混凝土模板温度控制在5~30℃(每孔梁浇注开盘前检测);入模温度为5~30℃(每批不大于100m 3测一次);混凝土入模含气量控制在2%~4%(每批不大于50m 3测一次);混凝土坍落度(坍落扩展度)每批不大于50m 3测一次。是什么意思?

待解决 悬赏分:1 - 离问题结束还有
混凝土模板温度控制在5~30℃(每孔梁浇注开盘前检测);入模温度为5~30℃(每批不大于100m 3测一次);混凝土入模含气量控制在2%~4%(每批不大于50m 3测一次);混凝土坍落度(坍落扩展度)每批不大于50m 3测一次。
问题补充:

  • 匿名
2013-05-23 12:21:38
正在翻译,请等待...
  • 匿名
2013-05-23 12:23:18
formwork temperature control in 5 to 30 °C Leung (each hole pour pre-opening testing); into the mold temperature to 5 ~ 30 (each batch of little °C to detect a ) 3 100 m; concrete into the mold containing gas volume control in 2 to 4 percent (each batch of less than 50 m 3 ) A detection; concrete 7-
  • 匿名
2013-05-23 12:24:58
The concrete template temperature control (pours in front of opening price in 5~30℃ each Kong Liang to examine); Enters the mold temperature (not to be bigger than 100m 3 for 5~30℃ each batch to measure one time); The concrete enters the mold air content control (not to be bigger than 50m 3 in 2%~4%
  • 匿名
2013-05-23 12:26:38
Concrete temperature control in the 5~30℃ (per Kong Liang cast before the opening test), into the die temperature of 5~30℃ (each consisting of not more than 100m 3 log); air content of concrete into the mold control in 2%~4% (each consisting of not more than 50m 3 log); slump of concrete (slump exte
  • 匿名
2013-05-23 12:28:18
Concrete temperature control in the 5~30℃ (per Kong Liang cast before the opening test), into the die temperature of 5~30℃ (each consisting of not more than 100m 3 log); air content of concrete into the mold control in 2%~4% (each consisting of not more than 50m 3 log); slump of concrete (slump exte
 
 