求翻译:As mineral additive, material uses crushed slag resulting from nickel production, said components are taken in the following ratio, wt.-%: Portland cement clinker, 76-80; gypsum, 4-5; crushed nickel slag, 15-20. EFFECT: reliable sealing of space around and behind drill pipe string; thermal stability for prolonged perio是什么意思?

待解决 悬赏分:1 - 离问题结束还有
As mineral additive, material uses crushed slag resulting from nickel production, said components are taken in the following ratio, wt.-%: Portland cement clinker, 76-80; gypsum, 4-5; crushed nickel slag, 15-20. EFFECT: reliable sealing of space around and behind drill pipe string; thermal stability for prolonged perio
问题补充:

  • 匿名
2013-05-23 12:21:38
作为矿物添加剂,材料使用从镍生产所得碎炉渣,所述组分都是在以下比例,重量 - % :波特兰水泥熟料, 76-80 ;
  • 匿名
2013-05-23 12:23:18
作为矿物添加剂,材料用途击碎了炉渣起因于镍生产,说组分在以下比率,重量被采取。- % :波特兰水泥粉煤渣, 76-80;石膏, 4-5;被击碎的镍炉渣, 15-20。作用:空间可靠的海豹捕猎在和在钻杆串后附近;长时间的耐热性;乏味孔支持和增加的产能延长的产品使用期限。
  • 匿名
2013-05-23 12:24:58
作为矿物添加剂,材料用途被击碎的炉渣起因于镍生产,认为组分在以下比率,重量被采取。- % : 波特兰水泥粉煤渣, 76-80; 石膏, 4-5; 被击碎的镍炉渣, 15-20。 作用: 空间可靠的海豹捕猎在和在钻杆串之后附近; 耐热性为长时间; 乏味孔支持和增加的生产能力延长的产品使用期限。
  • 匿名
2013-05-23 12:26:38
说: 组件所需的以下比例,由于矿物添加剂、 材料使用压碎渣产生的镍生产工艺,wt.-%: 波特兰水泥熟料,76-80 ;石膏、 4-5 ;被击碎的镍渣,15-20。效果: 周围的空间背后钻管柱 ; 密封可靠。热稳定性为长时间 ; 的延长的使用寿命的孔孔的支持和增加产能。
  • 匿名
2013-05-23 12:28:18
作为矿物质添加剂,材料因镍生产而产生使用被压碎的矿渣,组件说被欺骗以下比率, wt. %:普通水泥使发出叮当声者, 76-80 ;石膏, 4-5 ;被压倒镍矿渣, 15-20。效果:可靠空间的密封大约和在后面钻烟斗字符串;延长的时期的热稳定性;讨厌鬼孔支持的延续的服务一生和增强生产能力。
 
 