求翻译:The results show that the size of flash gutter bridge, the lubricating condition and the deformation process are the main factors influencing the filling qualities of complex-shape aluminum alloy forging. The folding defect is mainly caused by different velocities of filling cavities, fast flow of much metal in one di;是什么意思?

待解决 悬赏分:1 - 离问题结束还有
The results show that the size of flash gutter bridge, the lubricating condition and the deformation process are the main factors influencing the filling qualities of complex-shape aluminum alloy forging. The folding defect is mainly caused by different velocities of filling cavities, fast flow of much metal in one di;
问题补充:

  • 匿名
2013-05-23 12:21:38
该结果表明,飞边槽桥的大小,润滑状态和变形过程是影响的复杂形状的铝合金锻造的填充质量的主要因素。
  • 匿名
2013-05-23 12:23:18
结果表示,一刹那天沟桥梁的大小,润滑的情况和变形过程是影响复杂形状铝合金锻件的填装的质量的主要因素。折叠的瑕疵由不同的速度填装的洞主要造成,斋戒金属流程在一二的; ection和合流两或多金属子线。
  • 匿名
2013-05-23 12:24:58
一刹那天沟桥梁的大小,润滑的情况和变形过程是影响复杂形状铝合金锻件的填装的质量的主要因素的结果展示。 折叠的瑕疵由不同的速度填装的洞在一二主要造成,斋戒金属流程; ection和合流二或多金属子线。
  • 匿名
2013-05-23 12:26:38
结果显示,大小的 flash 装订线桥、 润滑条件和变形过程是主要影响因素复杂形状铝合金锻件的灌装素质。折叠缺陷主要引起不同速度的灌装腔,快速流通的多金属在一个 di ; 与汇流处的两个或多金属丝。
  • 匿名
2013-05-23 12:28:18
结果显示大小的闪光排水沟桥,加润滑油条件和变形过程是影响复杂形状铝合金伪造的为人装满质量的主要因素。可折叠的缺陷主要由填充洞的不同速率造成,在一个中很多玻璃液的快的流动二;外离子和二的汇合或多金属搁浅。
 
 