求翻译:所得复合镀层的厚度随预镀时间的减小而增大,这可能因为复合镀液中有表面活性剂的加入所导致。是什么意思?

待解决 悬赏分:1 - 离问题结束还有
所得复合镀层的厚度随预镀时间的减小而增大,这可能因为复合镀液中有表面活性剂的加入所导致。
问题补充:

  • 匿名
2013-05-23 12:21:38
The obtained composite coating thickness with the decrease of the pre-plating time increases, which may be caused by the surfactant in the composite plating bath.
  • 匿名
2013-05-23 12:23:18
The resulting composite coating on the thickness of the time with the pre-plated decrease and increase, and this may be because composite plated liquid surfactants in the join.
  • 匿名
2013-05-23 12:24:58
Obtained compound coating thickness along with plates the time to reduce in advance increases, this possible because compound plates in the fluid to have the surface active agent to join causes.
  • 匿名
2013-05-23 12:26:38
Thickness of composite coatings obtained with preplating time decreases and increases, either because the composite plating in the surfactant is added to the lead.